Abstract
In this work, LiCoPO4 nanoparticles were synthesized by supercritical fluid method using cobalt nitrate hexahydrate (Co(NO3)2 6H2O) and cobalt acetate tetrahydrate (C4H6CoO4 4H2O) as starting materials. The effect of starting materials on particle morphology, size, and the crystalline phase were investigated. The as-synthesized samples were systematically characterized by XRD, TEM, STEM, EDS, BET, and TG and charge-discharge measurements. In addition, Rietveld refinement analysis was performed. The electrochemical measurements of LiCoPO4 nanoparticles have shown differences in capacities depending on the starting materials used in the synthesis and the results have been discussed in this paper.
You have requested "on-the-fly" machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Show full disclaimer
Neither ProQuest nor its licensors make any representations or warranties with respect to the translations. The translations are automatically generated "AS IS" and "AS AVAILABLE" and are not retained in our systems. PROQUEST AND ITS LICENSORS SPECIFICALLY DISCLAIM ANY AND ALL EXPRESS OR IMPLIED WARRANTIES, INCLUDING WITHOUT LIMITATION, ANY WARRANTIES FOR AVAILABILITY, ACCURACY, TIMELINESS, COMPLETENESS, NON-INFRINGMENT, MERCHANTABILITY OR FITNESS FOR A PARTICULAR PURPOSE. Your use of the translations is subject to all use restrictions contained in your Electronic Products License Agreement and by using the translation functionality you agree to forgo any and all claims against ProQuest or its licensors for your use of the translation functionality and any output derived there from. Hide full disclaimer