Abstract
OBJECTIVE: To analyze the influence of the soft-start curing protocol in the degree of conversion of a nanohybrid composite.
METHODS: Ten specimens were prepared from the polymerization of the composite resin Llis using two protocols: conventional (1000 mW/cm² for 20 seconds) or gradual (250 mW/cm² for 20 seconds + 1000 mW/cm² for 15 seconds). Then, analyzes were performed using a spectrophotometer and data were subjected to Two-way ANOVA and Holm-Sidak test. The significance level was 5%.
RESULTS: There was no statistical difference between the average resin conversion degree of composite values in the base area and top for both curing protocols (p > 0.05).
CONCLUSION: Therefore, the use of soft-start curing protocol did not interfere in the degree of conversion of a nanohybrid composite.
You have requested "on-the-fly" machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Show full disclaimer
Neither ProQuest nor its licensors make any representations or warranties with respect to the translations. The translations are automatically generated "AS IS" and "AS AVAILABLE" and are not retained in our systems. PROQUEST AND ITS LICENSORS SPECIFICALLY DISCLAIM ANY AND ALL EXPRESS OR IMPLIED WARRANTIES, INCLUDING WITHOUT LIMITATION, ANY WARRANTIES FOR AVAILABILITY, ACCURACY, TIMELINESS, COMPLETENESS, NON-INFRINGMENT, MERCHANTABILITY OR FITNESS FOR A PARTICULAR PURPOSE. Your use of the translations is subject to all use restrictions contained in your Electronic Products License Agreement and by using the translation functionality you agree to forgo any and all claims against ProQuest or its licensors for your use of the translation functionality and any output derived there from. Hide full disclaimer