High purity of (99.999%) Nano grain size from both SrTiO3 and BaTiO3 was used to prepare the composites ceramic capacitors. The fabricated discs were sintered at 1300 ˚C, for 3 hours under static air. X-ray diffraction, thermo gravimetric and differential thermal analysis, sintering behavior, SEM and AFM were conducted to study its physical and microstructural behavior. The best results indicated at the combination (BaTiO3 72 -SrTiO3 28) Wt.%, after sintering as composites ceramic fabricated from nano powder.
You have requested "on-the-fly" machine translation of selected content from our databases. This functionality is provided solely for your convenience and is in no way intended to replace human translation. Show full disclaimer
Neither ProQuest nor its licensors make any representations or warranties with respect to the translations. The translations are automatically generated "AS IS" and "AS AVAILABLE" and are not retained in our systems. PROQUEST AND ITS LICENSORS SPECIFICALLY DISCLAIM ANY AND ALL EXPRESS OR IMPLIED WARRANTIES, INCLUDING WITHOUT LIMITATION, ANY WARRANTIES FOR AVAILABILITY, ACCURACY, TIMELINESS, COMPLETENESS, NON-INFRINGMENT, MERCHANTABILITY OR FITNESS FOR A PARTICULAR PURPOSE. Your use of the translations is subject to all use restrictions contained in your Electronic Products License Agreement and by using the translation functionality you agree to forgo any and all claims against ProQuest or its licensors for your use of the translation functionality and any output derived there from. Hide full disclaimer