© 2023 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). Notwithstanding the ProQuest Terms and Conditions, you may use this content in accordance with the terms of the License.

Abstract

Laser powder bed fusion (L-PBF) has attracted great interest in recent years due to its ability to produce intricate parts beyond the capabilities of traditional manufacturing processes. L-PBF processed biomedical implants are usually made of commercial pure titanium (CP-Ti) or its alloys. However, both alloys are naturally bio-inert, and thus reduce the formation of apatite as implants are put into the human body. Accordingly, in an attempt to improve the bioactivity of the materials used for making orthopedic implants, the present study decomposed fluorapatite material (FA, (Ca10(PO4)6F2)) into the form of nano-powder and mixed this powder with CP-Ti powder in two different ratios (99%Ti + 1%FA (Ti-1%FA) and 98%Ti + 2%FA (Ti-2%FA)) to form powder material for the L-PBF process. Experimental trials were conducted to establish the optimal processing conditions (i.e., laser power, scanning speed and hatching space) of the L-PBF process for the two powder mixtures and the original CP-Ti powder with no FA addition. The optimal parameters were then used to produce tensile test specimens in order to evaluate the mechanical properties of the different samples. The hardness of the various samples was also examined by micro-Vickers hardness tests. The tensile strength of the Ti-1%FA sample (850 MPa) was found to be far higher than that of the CP-Ti sample (513 MPa). Furthermore, the yield strength of the Ti-1%FA sample (785 MPa) was also much higher than that of the CP-Ti sample (472 MPa). However, the elongation of the Ti-1%FA sample (6.27 %) was significantly lower than that of the CP-Ti sample (16.17%). Finally, the hardness values of the Ti-1%FA and Ti-2%FA samples were around 63.8% and 109.4%, respectively, higher than that of the CP-Ti sample.

Details

Title
Mechanical Properties of Titanium/Nano-Fluorapatite Parts Produced by Laser Powder Bed Fusion
Author
Po-Kuan Wu 1   VIAFID ORCID Logo  ; Wei-Ting, Lin 2 ; Jia-Wei, Lin 3 ; Hong-Chuong Tran 3 ; Tsung-Yuan Kuo 3   VIAFID ORCID Logo  ; Chi-Sheng, Chien 1 ; Vi-Long Vo 3 ; Ru-Li, Lin 3 

 Department of Orthopaedics, Chi Mei Medical Center, No. 901 Zhonghua Rd., Yongkang District, Tainan 710, Taiwan 
 Department of Orthopaedics, Chi Mei Medical Center, No. 901 Zhonghua Rd., Yongkang District, Tainan 710, Taiwan; Department of Mechanical Engineering, Southern Taiwan University of Science and Technology, Tainan 710, Taiwan 
 Department of Mechanical Engineering, Southern Taiwan University of Science and Technology, Tainan 710, Taiwan 
First page
1502
Publication year
2023
Publication date
2023
Publisher
MDPI AG
e-ISSN
19961944
Source type
Scholarly Journal
Language of publication
English
ProQuest document ID
2779520410
Copyright
© 2023 by the authors. Licensee MDPI, Basel, Switzerland. This article is an open access article distributed under the terms and conditions of the Creative Commons Attribution (CC BY) license (https://creativecommons.org/licenses/by/4.0/). Notwithstanding the ProQuest Terms and Conditions, you may use this content in accordance with the terms of the License.